Abstract:
Coal-based humic acid has a rich aromatic structure and strong reactivity, making it an excellent precursor for preparing hard carbon anode materials in sodium-ion batteries. However, the commercial humic acids derived from coal mostly use weathered coal as the raw material. The structural uniformity of the raw materials is relatively poor, which is not conducive to large-scale production. Brown coal possesses abundant reserves and low cost. Using Xinjiang lignite as the raw material, employing catalytic degradation to depolymerize its macromolecular structure and produce regenerated humic acid. Subsequently, humic acid-based hard carbon is synthesized through low-temperature thermal treatment (holding at 420 ℃ for 2, 4, and 6 h) and high-temperature carbonization (1 400 ℃). Investigate the effects of low-temperature pyrolysis control strategies on the microcrystalline structure, pore structure, and surface chemical composition of humic acid-based hard carbon. Additionally, study the sodium storage capacity of different humic acid-based hard carbons using constant-current charge-discharge, constant-current intermittent titration, and cyclic voltammetry testing methods. The results show that during the low-temperature heat treatment process, humic acid forms a cross-linked structure with C—O—C bridges between molecules, effectively inhibiting its tendency to graphiteification in the subsequent high-temperature heat treatment process. Compared with the samples that were not regulated by low-temperature pyrolysis, the humic acid-based hard carbon prepared through low-temperature treatment exhibits a larger carbon layer spacing and a higher content of amorphous carbon (including disordered carbon and pseudo-graphite carbon), while the defect concentration is reduced. When used as the negative electrode material for sodium-ion batteries, the samples obtained through low-temperature heat treatment exhibit higher reversible specific capacity, initial Coulombic efficiency, and superior rate performance and cycle stability. The raw material was held at 420 ℃ for 4 hours, then processed at 1 400 ℃ to produce sample HA-4h-1400, which exhibited the best sodium storage performance. Its reversible specific capacity at a current density of 0.02 A/g reached 265 mAh/g, with an initial Coulombic efficiency of 78.5%, and it still maintained a reversible specific capacity of 184 mAh/g at a current density of 1.0 A/g, demonstrating excellent rate performance.